A cylindrical rod of diameter 6.7 mm fabricated from a 70Cu-30Zn brass alloy is subjected to rotating-bending

Question:

A cylindrical rod of diameter 6.7 mm fabricated from a 70Cu-30Zn brass alloy is subjected to rotating-bending load cycling; test results (as S-N behavior) are shown in Figure 8.20. If the maximum and minimum loads are +120 N and -120 N, respectively, determine its fatigue life. Assume that the separation between load bearing points is 67.5 mm?

Fantastic news! We've Found the answer you've been seeking!