Is it possible to produce an iron-carbon alloy of eutectoid composition that has a minimum hardness of

Question:

Is it possible to produce an iron-carbon alloy of eutectoid composition that has a minimum hardness of 90 HRB and a minimum ductility of 35%RA? If so, describe the continuous cooling heat treatment to which the alloy would be subjected to achieve these properties. If it is not possible, explain why.
Fantastic news! We've Found the answer you've been seeking!

Step by Step Answer:

Related Book For  book-img-for-question

Materials Science and Engineering An Introduction

ISBN: 978-0470419977

8th edition

Authors: William D. Callister Jr., David G. Rethwisch

Question Posted: