A blast furnace makes pig iron containing 3 . 2 % and 1 . 8 % of Carban and Silicon and remaining as Iron respectively.

A blast furnace makes pig iron containing 3.2% and 1.8% of Carban and Silicon and remaining as Iron respectively. The ore is a combination of 80%,12% and 8% of Iron Oxide, Silica and Aluminum Oxide respectively. The process requires cake at a rate of 1Kg per kg of pig iron produced. The coke is adulterated with Silica with 10% of silica and remaining to be carbon. The flux is obtained at a rate of 0.4kg per kg of pig iron and is containing pure Calcium carbonate. The blast furnace gas has 30%CO and 15%CO2. Considering the base of one tonne of pig iron produced, calculate the following assuming the necessary data required:
The weight of core used.
The weight of slag made.
The volume of the blast-furnace gas.
image text in transcribed

Step by Step Solution

There are 3 Steps involved in it

Step: 1

blur-text-image

Get Instant Access to Expert-Tailored Solutions

See step-by-step solutions with expert insights and AI powered tools for academic success

Step: 2

blur-text-image

Step: 3

blur-text-image

Ace Your Homework with AI

Get the answers you need in no time with our AI-driven, step-by-step assistance

Get Started

Recommended Textbook for

Introduction To Chemical Engineering Thermodynamics

Authors: H.C. Smith, J.M. & Van Ness

2nd Edition

0070586993, 978-0070586994

More Books

Students also viewed these Chemical Engineering questions