Answered step by step
Verified Expert Solution
Link Copied!

Question

1 Approved Answer

An injection-moulded part is made with polypropylene reinforced with 15% glass fibres. The part is failing in tension during use. You examine the fracture surface

image text in transcribed

An injection-moulded part is made with polypropylene reinforced with 15% glass fibres. The part is failing in tension during use. You examine the fracture surface of the part and see the following. Fig.2 - Scanning electron microscope photo of bundles of glass fibres seen at a fracture surface. Comment on what can be done to improve the tensile properties of the part. In your analysis, comment on all aspects of the problem: polymer, glass properties, glass level, and compounding

Step by Step Solution

There are 3 Steps involved in it

Step: 1

blur-text-image

Get Instant Access to Expert-Tailored Solutions

See step-by-step solutions with expert insights and AI powered tools for academic success

Step: 2

blur-text-image

Step: 3

blur-text-image

Ace Your Homework with AI

Get the answers you need in no time with our AI-driven, step-by-step assistance

Get Started

Recommended Textbook for

Mass And Heat Transfer Analysis Of Mass Contactors And Heat Exchangers

Authors: T. W. Fraser Russell, Anne Skaja Robinson, Norman J. Wagner

1st Edition

0521886708, 9780521886703

More Books

Students also viewed these Chemical Engineering questions

Question

How We Listen?

Answered: 1 week ago