The tensile 0.2 percent offset yield strength of AISI 1137 cold-drawn steel rounds up to 1 inch

Question:

The tensile 0.2 percent offset yield strength of AISI 1137 cold-drawn steel rounds up to 1 inch in diameter from 2 mills and 25 heats is reported histographically as follows:

93 95 97 99 101 03 105 107 109 f19 25 38 17 12 10 54 4 2


Where Sy is the class midpoint in kpsi and f is the number in each class. Presuming the distribution is normal, what is the yield strength exceeded by 99 percent of the population?

Distribution
The word "distribution" has several meanings in the financial world, most of them pertaining to the payment of assets from a fund, account, or individual security to an investor or beneficiary. Retirement account distributions are among the most...