Nickel containing 2 wt% thorium is produced in powder form, consolidated into a part, and sintered in

Question:

Nickel containing 2 wt% thorium is produced in powder form, consolidated into a part, and sintered in the presence of oxygen, causing all of the thorium to produce ThO2 spheres 80 nm in diameter. Calculate the number of spheres per cm3. The density of ThO2 is 9.69 g/cm3.