Spherical aluminum powder (SAP) 0.002 mm in diameter is treated to create a thin oxide layer and

Question:

Spherical aluminum powder (SAP) 0.002 mm in diameter is treated to create a thin oxide layer and is then used to produce a SAP dispersion-strengthened material containing 10 vol% Al2O3. Calculate the average thickness of the oxide film prior to compaction and sintering of the powders into the part.
Fantastic news! We've Found the answer you've been seeking!

Step by Step Answer:

Related Book For  book-img-for-question

Essentials of Materials Science and Engineering

ISBN: 978-1111576851

3rd edition

Authors: Donald R. Askeland, Wendelin J. Wright

Question Posted: