Freckling of superalloy ingots. Freckles are defects that sometimes form during the solidification of alloy ingots. A
Question:
Freckling of superalloy ingots. Freckles are defects that sometimes form during the solidification of alloy ingots.
A freckle index has been developed to measure the level of freckling on the ingot. A team of engineers conducted several experiments to measure the freckle index of a certain type of superalloy (Journal of Metallurgy, Sept.
2004). The data for n = 18 alloy tests are shown in the table.
a. Construct a box plot for the data and use it to find any outliers.
b. Find and interpret the z-scores associated with the alloys you identified in part a.