For a steel alloy it has been determined that a carburizing heat treatment of 10.3h duration will raise the carbon concentration to 0.320wt% at a
For a steel alloy it has been determined that a carburizing heat treatment of 10.3h duration will raise the carbon concentration to 0.320wt% at a point 1.20mm from the surface. Estimate the time necessary to achieve the same concentration at a 4.90mm position for an identical steel and at the same carburizing temperature. t= h