Monomer M is to be polymerized using a peroxide initiator, I. The peroxide has a half-life of 6.00h at 70oC. The polymerization is to be
Monomer M is to be polymerized using a peroxide initiator, I. The peroxide has a half-life of 6.00h at 70oC. The polymerization is to be carried out with the following requirements: Polymerization time: 2.00 min
Polymerization temperature: 70oC
Conversion: 2.00% Initial degree of polymerization: 1200
If the initiation efficiency (f) = 1.00, and termination is by coupling, what concentration of peroxide should be used (in mol peroxide/mol of monomer)?