A niobium alloy is produced by introducing tungsten substitutional atoms in the BCC structure; eventually an alloy

Question:

A niobium alloy is produced by introducing tungsten substitutional atoms in the BCC structure; eventually an alloy is produced that has a lattice parameter of 0.32554 nm and a density of 11.95 g/cm3. Calculate the fraction of the atoms in the alloy that are tungsten.